Medalist® MD-12180 (PRELIMINARY DATA)

注: 该材料由 TEKNOR APEX 厂家直供,厂家技术人员进行生产指导,提供正规出场报告,相关检测报告等。

种类 :TPE
品牌 :Medalist™
用途 : 医疗/护理用品垫圈药物插头外壳橡胶取代柔软的把手旋钮衬套Disposable Hospital Goods

Medalist® MD-12180 (PRELIMINARY DATA) 原厂PDF物性资料.pdf

 订购热线:021-58958519 13061808058(赵先生)

Medalist® MD-12180 (PRELIMINARY DATA) 产品信息
基本信息
特性
  • Low Specific Gravity
  • Without Fillers
  • 低密度
  • 辐射消毒
  • 高压锅消毒
  • 光滑性
  • 好的消毒性
  • 环氧乙烷消毒
  • 良好的成型性能
  • 良好粘结性
  • 流动性中等
  • 耐化学性良好
  • 韧性良好
  • 润滑
  • 无卤
  • 硬度高
  • 有弹性
用途
  • Disposable Hospital Goods
  • 插头
  • 衬套
  • 垫圈
  • 柔软的把手
  • 外壳
  • 橡胶取代
  • 旋钮
  • 药物
  • 医疗/护理用品
机构评级
  • ISO 10993 Part 5
  • ISO 13485
RoHS 合规性
  • RoHS 合规
外观
  • 半透明
  • 可用颜色
  • 自然色
形式
  • 粒子
加工方法
  • 注射成型
物理性能额定值单位制测试方法
比重 0.891g/cm³ASTM D792
熔流率(熔体流动速率) (200°C/5.0 kg)9.0g/10 minASTM D1238
硬度额定值单位制测试方法
肖氏硬度 ASTM D2240
    邵氏 A, 1 秒 82ASTM D2240
    邵氏 A, 5 秒 80ASTM D2240
弹性体额定值单位制测试方法
拉伸应力 1ASTM D412
    50%应变 3.79MPaASTM D412
    100%应变 4.27MPaASTM D412
    300%应变 5.45MPaASTM D412
抗张强度 2(断裂)12.0MPaASTM D412
伸长率 3(断裂)720%ASTM D412
撕裂强度 450.3kN/mASTM D624
压缩永久变形 5ASTM D395
    23°C, 22 hr 25%ASTM D395
    70°C, 22 hr 44%ASTM D395
法律声明
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
注射额定值单位制
料筒后部温度 160 到 177°C
料筒中部温度 182 到 204°C
料筒前部温度 193 到 216°C
射嘴温度 182 到 227°C
加工(熔体)温度 182 到 227°C
模具温度 27 到 49°C
注射速度 中等偏快
背压 0.172 到 0.689MPa
螺杆转速 50 到 100rpm
垫层 3.81 到 12.7mm
注射说明
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
备注
1 .C 模具, 510 mm/min
2 .C 模具, 510 mm/min
3 .C 模具, 510 mm/min
4 .C 模具, 510 mm/min
5 .类型 1