Sarlink® TPE ME-2655B (PRELIMINARY DATA)

注: 该材料由 TEKNOR APEX 厂家直供,厂家技术人员进行生产指导,提供正规出场报告,相关检测报告等。

种类 :TPE
品牌 :Sarlink® TPE
用途 : 汽车领域的应用汽车外部零件橡胶取代车窗封装

Sarlink® TPE ME-2655B (PRELIMINARY DATA) 原厂PDF物性资料.pdf

 订购热线:021-58958519 13061808058(赵先生)

Sarlink® TPE ME-2655B (PRELIMINARY DATA) 产品信息
基本信息
特性
  • Low Specific Gravity
  • 出色的外观
  • 低密度
  • 抗紫外线性能良好
  • 可加工性,良好
  • 良好粘结性
  • 流动性高
  • 耐化学性良好
  • 有弹性
  • 中等硬度
用途
  • 车窗封装
  • 汽车领域的应用
  • 汽车外部零件
  • 橡胶取代
RoHS 合规性
  • RoHS 合规
外观
  • 黑色
形式
  • 粒子
加工方法
  • 注射成型
物理性能额定值单位制测试方法
密度 0.939g/cm³ISO 1183
熔流率(熔体流动速率) (190°C/2.16 kg)6.4g/10 minASTM D1238
硬度额定值单位制测试方法
肖氏硬度 ISO 868
    邵氏 A, 1 秒 60ISO 868
    邵氏 A, 5 秒 57ISO 868
    邵氏 A, 15 秒 55ISO 868
弹性体额定值单位制测试方法
拉伸应力 ISO 37
    横向流量 : 100%应变 1.56MPaISO 37
    流量 : 100%应变 1.94MPaISO 37
抗张强度 ISO 37
    横向流量 : 断裂 10.5MPaISO 37
    流量 : 断裂 7.80MPaISO 37
伸长率 ISO 37
    横向流量 : 断裂 880%ISO 37
    流量 : 断裂 770%ISO 37
撕裂强度
    横向流量 23kN/mISO 34
    流量 23kN/mISO 34-1
压缩永久变形 ISO 815
    23°C, 22 hr 17%ISO 815
    70°C, 22 hr 36%ISO 815
    90°C, 70 hr 61%ISO 815
老化额定值单位制测试方法
空气中拉伸强度的变化率 - 横向流量 ISO 188
    110°C, 1008 hr 8.7%ISO 188
    125°C, 168 hr 5.4%ISO 188
在空气中断裂时拉伸应力变化 - 横向流量 ISO 188
    110°C, 1008 hr 3.4%ISO 188
    125°C, 168 hr 1.4%ISO 188
空气中邵氏硬度的变化率 ISO 188
    邵氏 A, 110°C, 1008 hr 1.3ISO 188
    邵氏 A, 125°C, 168 hr 2.1ISO 188
补充信息额定值单位制测试方法
Apparent Shear Viscosity - Capillary, 206 1/sec (200°C)139Pa·sISO 11443
Good adhesion to glass with primer
法律声明
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
注射额定值单位制
料筒后部温度 170 到 190°C
料筒中部温度 175 到 195°C
料筒前部温度 180 到 205°C
射嘴温度 180 到 205°C
加工(熔体)温度 180 到 205°C
模具温度 15 到 40°C
注塑压力 1.38 到 6.89MPa
注射速度 中等偏快
背压 0.172 到 0.862MPa
螺杆转速 50 到 100rpm
垫层 3.81 到 25.4mm
注射说明
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 176°F (80°C).